An international round-robin calibration protocol for nanoindentation measurements

M. Cabibbo*, P. Ricci, R. Cecchini, Z. Rymuza, J. Sullivan, S. Dub, S. Cohen

*Corresponding author for this work

Research output: Contribution to journalArticle