Skip to main navigation Skip to search Skip to main content

Low-carbon cementitious grouts with straw biochar and ladle furnace slag: A micro- to macro-scale investigation

Research output: Contribution to journal › Article › peer-review

8   Link opens in a new tab Citations (SciVal)
15 Downloads (Pure)

Abstract

Combining agricultural and industrial-derived wastes offers a promising strategy to develop low-carbon cementitious materials. In this study, twelve cementitious grout formulations incorporating straw biochar (BC), fly ash (FA), and ladle furnace slag (LFS) were designed for application in grouted macadam pavements. The grouts were characterised in terms of fresh properties (flow spread, efflux time, and bleeding), hardened performance (mechanical properties, drying shrinkage, and water penetrability parameters), and microstructural features (hydration kinetics, XRD, TGA, and SEM-EDS). In addition, sustainability impacts were briefly assessed by considering only the material production stage, encompassing cost, embodied carbon, and energy. The results show that BC contents up to 15% can be effectively incorporated into ternary grout systems while meeting workability requirements, whereas higher BC dosages (25%) markedly increase viscosity and reduce flowability. BC-containing mixes exhibited comparable 3-day compressive strength (fc) to other blended systems under water curing, likely due to micro-filler effects, but reduced fc at longer ages because of clinker dilution and limited chemical reactivity. Nevertheless, mixes containing ≥ 70% Portland cement (PC) with 15% BC achieved an acceptable 28-day fc (≥40 MPa). Under air curing, all mixes showed strength reductions relative to water curing; however, BC-modified systems experienced lower strength losses (at least 20%) than BC-free mixes, likely benefiting the potential BC internal-curing effect. Flexural strength was maintained in BC-modified grouts, particularly when combined with LFS, even at reduced PC contents. Although high BC content generally increased water absorption and drying shrinkage due to its intrinsic porosity, FA partially improved dimensional stability. Simplified material-level sustainability analysis showed that ternary mixes with 15% BC plus 15% LFS reduced the normalized embodied carbon per flexural and compressive strength units by 66% and 40%, respectively, suggesting the suitability for semi-structural low-carbon applications.
Original languageEnglish
Article number146662
Number of pages21
JournalConstruction and Building Materials
Volume531
Early online date18 May 2026
DOIs
Publication statusPublished - 11 Jul 2026

Bibliographical note

Copyright © 2026 The Author(s). Published by Elsevier Ltd. This is an open access article under the CC BY license (https://creativecommons.org/licenses/by/4.0/).

Funding

The authors express their gratitude to the UK Research and Innovation (UKRI)—Innovate UK for the financial support received under the scope of the Knowledge Transfer Partnerships program (KTP No. 13622) between Aston University and Miles Macadam Ltd.

FundersFunder number
UK Research and Innovation
Miles Macadam Ltd
Aston University
Innovate UK13622

    Keywords

    • Bio-based composites
    • Flow spread and time
    • Mechanical and microstructural characterization
    • Material sustainability impacts
    • Supplementary cementitious materials

    Fingerprint

    Dive into the research topics of 'Low-carbon cementitious grouts with straw biochar and ladle furnace slag: A micro- to macro-scale investigation'. Together they form a unique fingerprint.

    Cite this